Pemco Frit P-926

Alternate Names: Frit 926, Frit P926

Description: Leadless fast fire frit

Oxide Analysis Formula Tolerance
CaO 17.00% 0.68
K2O 0.30% 0.01
Na2O 8.50% 0.31
B2O3 18.70% 0.61
Al2O3 5.00% 0.11
SiO2 50.50% 1.90
Oxide Weight 225.57
Formula Weight 225.57

Notes

Replaced P-54 in wall tile industry. It has lower solubility to prevent thickening or 'set' in glaze slurries.

Related Information

Links

Materials Ferro Frit 3288
Materials Fusion Frit F-13
Materials Pemco Frit P-1R63
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Pemco Frit P-54
Materials General Frit GF-103
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.4 x 10-6 (50-450C)
Frit Melting Range (C) 1650-1700F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy