Ferro Frit 3288

Description: Sodium calcium borosilicate frit for wall tile glazes

Oxide Analysis Formula Tolerance
CaO 16.91% 0.68
K2O 0.42% 0.01
Na2O 8.52% 0.31
B2O3 18.82% 0.61
Al2O3 4.97% 0.11
SiO2 50.36% 1.89
Oxide Weight 225.58
Formula Weight 225.58

Notes

Same formula as Ferro 3814 but made from different materials.

Related Information

Links

Materials Pemco Frit P-926
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-103
Materials Fusion Frit F-13
Materials Ferro Frit 3814
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.80
Frit Softening Point 1800F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy