Narco Fireclay

Oxide Analysis Formula Tolerance
CaO 0.13% 0.01
K2O 2.20% 0.08
MgO 0.60% 0.05
Na2O 0.30% 0.02
TiO2 1.75% 0.07
Al2O3 31.20% 1.00
SiO2 52.70% 2.87
Fe2O3 1.84% 0.04
LOI 9.58%n/a
Oxide Weight 296.58
Formula Weight 328.01

Notes

Low plasticity fireclay, good for sculpture. Very refractory (10% absorption, 12% total shrinkage at cone 10)

Related Information

Links

Materials Fireclay
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy