Formula: KAl2(Si3Al)O10(OH,F)2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 11.80% | 1.00 | |
| Al2O3 | 38.36% | 3.00 | |
| SiO2 | 45.21% | 6.01 | |
| F | 0.95% | 0.40 | |
| LOI | 4.07% | n/a | |
| Oxide Weight | 768.93 | ||
| Formula Weight | 801.55 | ||

This picture has its own page with more detail, click here to see it.
Aquamarine Muscovite Albite

This picture has its own page with more detail, click here to see it.
Almand Cleveland Muscov-ite

This picture has its own page with more detail, click here to see it.
Muscovite Stone2

This picture has its own page with more detail, click here to see it.
Muscovite Mica
| URLs |
http://www.webmineral.com/data/Muscovite.shtml
Muscovite at webmineral.com |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |