| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Li2O | 7.10% | 0.94 | |
| K2O | 0.60% | 0.03 | |
| Na2O | 0.30% | 0.02 | |
| P2O5 | 0.40% | 0.01 | |
| Al2O3 | 25.00% | 0.97 | |
| Fe2O3 | 0.15% | - | |
| MnO2 | 0.06% | - | |
| SiO2 | 66.20% | 4.37 | |
| LOI | 0.20% | n/a | |
| Oxide Weight | 395.63 | ||
| Formula Weight | 396.42 | ||
| Materials |
Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O. |