Hommel Frit K-3

Alternate Names: Frit K3

Description: Leadless Frit

Oxide Analysis Formula Tolerance
CaO 6.77% 0.33
Na2O 15.12% 0.67
B2O3 21.87% 0.86
SiO2 56.23% 2.57
Oxide Weight 274.28
Formula Weight 274.28

Related Information

Links

Materials Ferro Frit 3278
Materials Fusion Frit F-60
Materials Pemco Frit P-830
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-109
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.5 x 10-6 (50-450C)
Co-efficient of Linear Expansion 8.5 x 10-6
Frit Softening Point 1450F
Frit Melting Range (C) 1450F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy