Ferro Frit 3278

Alternate Names: F3278

Description: Leadless high boron calcia alkali silicate frit

Oxide Analysis Formula Tolerance
CaO 6.86% 0.33
Na2O 15.10% 0.67
B2O3 21.73% 0.85
SiO2 56.31% 2.56
Oxide Weight 273.35
Formula Weight 273.35

Notes

This is a USA pottery frit, Ferro now calls it Frit 3278-2.

It is high in alkali and thus has a high thermal expansion. Useful in partially fritted wall tile glazes cone 08-02.

Related Information

Links

Materials Pemco Frit P-830
Materials Fusion Frit F-60
Materials Hommel Frit K-3
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials General Frit GF-109
Materials Ferro Frit 3270
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
URLs https://digitalfire.com/4sight/datasheets/ferropotteryfrits2008.pdf
Ferro Pottery Frits 2008

Data

Co-efficient of Linear Expansion 9.7
Frit Melting Range (C) 1400-1550F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy