Alternate Names: Frit 830, Frit P830
Description: Leadless Frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 7.20% | 0.35 | |
| Na2O | 14.90% | 0.65 | |
| B2O3 | 21.60% | 0.84 | |
| SiO2 | 56.30% | 2.54 | |
| Oxide Weight | 271.25 | ||
| Formula Weight | 271.25 | ||
| Materials |
Ferro Frit 3278
|
| Materials |
Fusion Frit F-60
|
| Materials |
Hommel Frit K-3
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
General Frit GF-109
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.6 x 10-6 (50-450C) |
|---|---|
| Frit Melting Range (C) | 1320-1420F |