Alternate Names: Frit 143, Frit GF143
Description: Sodium Boron Silicate Leadless
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 8.48% | 1.00 | |
| B2O3 | 38.48% | 4.04 | |
| SiO2 | 53.04% | 6.45 | |
| Oxide Weight | 731.13 | ||
| Formula Weight | 731.13 | ||
A 'specific-oxide' borosilicate frit (contains only sodium, boron, silica).
Used to bond abrasives.
| Materials |
Ferro Frit 3185
|
| Materials |
Fusion Frit F-245
|
| Materials |
Ferro Frit 3226
|
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Fusion Frit F-367
|
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 6.40 |
|---|---|
| Frit Softening Point | 1750F |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk