1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Fusion Frit F-245

Alternate Names: Fusion Frit F245

Description: Alkali boron bonding frit

Oxide Analysis Formula Tolerance
CaO 3.00% 0.31
Na2O 7.30% 0.69
B2O3 36.40% 3.05
Al2O3 0.90% 0.05
SiO2 52.40% 5.09
Oxide Weight 584.05
Formula Weight 584.05

Related Information

Links

Materials Ferro Frit 3185
Materials General Frit GF-143
Materials Ferro Frit 3226
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.
Typecodes Bonding Frits
Also called glass frits, these melt at very low temperatures (e.g. 500C). They are used to bond together materials that can withstand some heat (e.g. abrasives, ceramics, non-oxide ceramics, metals). And as a surface-smoothing agent. The main product properties are melting temperature and thermal expansion. The powders are mixed with binders, applied and then heated up and down to create the bond.

Data

Co-efficient of Linear Expansion 4.61
Frit Softening Point 1550F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy