G-200 2R Feldspar

Oxide Analysis Formula Tolerance
SiO2 66.50% 6.71 1
Al2O3 18.20% 1.08 1
Fe2O3 0.10% -
K2O 11.00% 0.71
Na2O 2.50% 0.24 .75
CaO 0.30% 0.03
MgO 0.10% 0.02
LOI 0.30%n/a
Oxide Weight 598.46
Formula Weight 600.26

Notes

From an IMERYS mine in India. Hammill and Gillespie are importing it and are confident that the level of quality is good and it has almost the same chemistry as the G200 EU. They have product for testing in New Jersey (early 2024). The lead-time to a West Coast port is 10 to 12 weeks. It seems to have an impossibly low Fe2O3 content.

Available in 20, 40, 50 kg bags and 800,1000,1200,1250,1350 kg bulk bags.

Related Information

Links

Materials Feldspar
In ceramics, feldspars are used in glazes and clay bodies. They vitrify stonewares and porcelains. They supply KNaO flux to glazes to help them melt.
Materials G-200 EU Feldspar
Materials G-200 Feldspar
Materials G200 HP Feldspar
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
URLs https://digitalfire.com/4sight/datasheets/G200-HR.pdf
G-200 2R Data Sheet

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy