Description: G200 equivalent from Spain
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 68.50% | 7.06 | |
| Al2O3 | 17.00% | 1.03 | |
| Fe2O3 | 0.10% | - | |
| TiO2 | 0.03% | - | |
| K2O | 11.00% | 0.72 | |
| Na2O | 2.10% | 0.21 | |
| CaO | 0.50% | 0.06 | |
| MgO | 0.08% | 0.01 | |
| LOI | 0.50% | n/a | |
| Oxide Weight | 614.76 | ||
| Formula Weight | 617.85 | ||
This is being sold by Imerys as an equivalent to G200 Feldspar (because the mine of the latter is being closed during 2013 because the deposit is depleted). The data sheet says it is obtained from a feldspathic sand by a flotation process.
It is 70% K Feldspar, 23% Na Feldspar, 7% quartz.
Particle size:
+200 mesh: 0.5%
+325 mesh: 6.2%
On paper the chemistry is pretty similar to G-200.
Laguna Clay is now selling Mahavir Feldspar from India as the G200 equivalent.
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Materials |
G-200 Feldspar
|
| Materials |
G200 Old Blend Feldspar
|
| Materials |
Mahavir Potash Feldspar
|
| Materials |
G-200 2R Feldspar
|
| URLs |
https://digitalfire.com/4sight/datasheets/G-200-EU.pdf
G-200-EU Datasheet |