FinnTalc

Description: Hydrous Magnesium Calcium Silicate

Oxide Analysis Formula Tolerance
MgO 31.00% 1.00
Al2O3 0.20% -
SiO2 61.00% 1.32
FeO 1.90% 0.03
LOI 5.40%n/a
Oxide Weight 122.33
Formula Weight 129.31

Related Information

Links

Materials Talc
A source of MgO for ceramic glazes, a flux or thermal expansion additive in clay bodies, also used in the manufacture of cordierite.
Hazards Talc Hazards Overview
Talc is invaluable in the ceramics industry, it is used as a glaze and body ingredient and as a parting a release agent in various processes. Is it safe?
URLs http://www.mondominerals.com/uploads/tx_drivemondoproducts/FINNTALC_M20SL-AW.pdf
FinnTalc M20SL Data Sheet

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy