Feldspath ICE 10

Oxide Analysis Formula Tolerance
K2O 10.00% 0.67
Na2O 2.70% 0.28
CaO 0.20% 0.02
MgO 0.10% 0.02
P2O5 0.30% 0.01
Fe2O3 0.10% -
Al2O3 17.30% 1.07
SiO2 69.20% 7.29
LOI 0.65%n/a
Oxide Weight 632.81
Formula Weight 636.95

Related Information

Links

Materials Feldspar
In ceramics, feldspars are used in glazes and clay bodies. They vitrify stonewares and porcelains. They supply KNaO flux to glazes to help them melt.
Hazards Feldspar
Feldspars are abundant and varied in nature. They contain small amounts of quartz (while nepheline syenite does not).
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy