Monthly Tech-Tip | No tracking! No ads! |
Oxide | Analysis | Formula | Tolerance |
---|---|---|---|
SiO2 | 99.30% | 337.06 | |
Al2O3 | 0.50% | 1.00 | .05 |
Fe2O3 | 0.04% | 0.05 | max |
Na2O | 0.01% | 0.03 | max |
CaO | 0.01% | 0.04 | .0005 |
TiO2 | 0.03% | 0.08 | max |
LOI | 0.15% | n/a | |
Oxide Weight | 20,377.56 | ||
Formula Weight | 20,408.17 |
A high quality silica sand suitable for producing glass containers, fiberglass insulation and specialized glaze making. This comes from the same quarry as EP Kaolin.
Materials |
EP Kaolin
A kaolin that gels slurries (thus handy to suspend ceramic glazes). It is plastic and fires white enough that it is also valuable in porcelain bodies. |
Materials |
Glass Sand
|
Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
URLs |
http://edgarminerals.com/Glass-Sand.html
Edgar Glass sand web page |
Bulk Density lbs/cu. ft. (Packed) | 95 |
---|---|
Sieve Analysis Dry | +40 mesh: 1.4% +50: 9.0 +70: 20.4 +100: 46.6 +140: 18.5 |
By Tony Hansen Follow me on ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() | ![]() |
Buy me a coffee and we can talk