Alternate Names: Ceraclay LPC
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.05% | - | |
| K2O | 2.20% | 0.06 | |
| MgO | 0.25% | 0.02 | |
| Na2O | 0.10% | - | |
| TiO2 | 0.04% | - | |
| Al2O3 | 37.50% | 1.00 | |
| SiO2 | 47.00% | 2.13 | |
| Fe2O3 | 0.90% | 0.02 | |
| LOI | 11.90% | n/a | |
| Oxide Weight | 239.47 | ||
| Formula Weight | 271.81 | ||
Particle Size Distribution:
>53 microns: 1.0 max
>10 microns: 20
<2 microns: 30
Modulus of Rupture, Kgf/cm2:
At 80% Relative Humidity: 4.0
Dried at 110C: 7.0
Casting Rate @ 65% solids (mm2/min): 4.0
% P84 Deflocculant Required for 5 Poise Slip: 0.5
1180C 1280C
Fired Absorption: 18% 10%
Fired Shrinkage: 6.5% 10%
Brightness: 84 86
| Minerals |
Mica
See Muscovite. |
| Minerals |
Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How |
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |