General Frit GF-103

Alternate Names: Frit 103, Frit GF103

Description: Calcium sodium borosilicate for partially fritted tile glazes

Oxide Analysis Formula Tolerance
CaO 16.91% 0.68
K2O 0.42% 0.01
Na2O 8.52% 0.31
B2O3 18.82% 0.61
Al2O3 4.97% 0.11
SiO2 50.36% 1.89
Oxide Weight 225.58
Formula Weight 225.58

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3288
Materials Fusion Frit F-13
Materials Hommel Frit 550
Materials Pemco Frit P-926
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 8.80
Frit Softening Point 1800F