Description: Very high sodium, boron free, high expansion frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 28.89% | 1.00 | |
| Al2O3 | 9.51% | 0.20 | |
| SiO2 | 61.61% | 2.20 | |
| Oxide Weight | 214.63 | ||
| Formula Weight | 214.63 | ||
Commonly used to make crystalline glazes because of the high sodium and relatively low alumina (Al2O3) contents. However other similar frits have much lower Al2O3.
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Materials |
Fusion Frit F644
|
| Materials |
Mondre and Manz Frit 1233
|
| Materials |
Glasurfritten M1233
|
| Materials |
Moulin Fritte M1233
|
| Materials |
Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts a very low temperatures. |
| Co-efficient of Linear Expansion | 123 x 10-7 (20-400C) |
|---|---|
| Heating Microscope Analysis for Frits | 458C |
| Heating Microscope Analysis for Frits | 685C |
| Heating Microscope Analysis for Frits | 890C |