Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Please don't panic, I am overwhelmed by the unbelievable support I am getting. We just need to get them to relent on this demand and call off the lawyer (to at least permit commentary). There are lots of backup sites (many people have the API endpoints), don't start downloading or scraping again and overload the server.
Insight-live.com general operation is not affected by this.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 55.38% | 2.20 | |
| Al2O3 | 42.69% | 1.00 | |
| Fe2O3 | 0.33% | - | |
| TiO2 | 0.06% | - | |
| CaO | 0.06% | - | |
| MgO | 0.21% | 0.01 | |
| K2O | 1.15% | 0.03 | |
| Na2O | 0.12% | - | |
| Oxide Weight | 238.93 | ||
| Formula Weight | 238.93 | ||
| Minerals |
Mica
See Muscovite. |
| Minerals |
Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Glossary |
Calcination
Calcining is simply firing a ceramic material to create a powder of new physical properties. Often it is done to kill the plasticity or burn away the hydrates, carbonates, sulfates of a clay or refractory material. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk