Edgar Glass Sand

Oxide Analysis Formula Tolerance
SiO2 99.30% 337.06
Al2O3 0.50% 1.00 .05
Fe2O3 0.04% 0.05 max
Na2O 0.01% 0.03 max
CaO 0.01% 0.04 .0005
TiO2 0.03% 0.08 max
LOI 0.15%n/a
Oxide Weight 20,377.56
Formula Weight 20,408.17

Notes

A high quality silica sand suitable for producing glass containers, fiberglass insulation and specialized glaze making. This comes from the same quarry as EP Kaolin.

Related Information

Links

Materials EP Kaolin
A kaolin that gels slurries (good for suspending glazes). It has two variations: a low and medium plasticity. It fires white for use in porcelain bodies.
Materials Glass Sand
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.
URLs http://edgarminerals.com/Glass-Sand.html
Edgar Glass sand web page

Data

Bulk Density lbs/cu. ft. (Packed) 95
Sieve Analysis Dry +40 mesh: 1.4% +50: 9.0 +70: 20.4 +100: 46.6 +140: 18.5

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy