Alternate Names: Feldspat 645
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.77% | 0.09 | |
| MgO | 0.05% | 0.01 | |
| K2O | 0.48% | 0.03 | |
| Na2O | 8.50% | 0.87 | |
| TiO2 | 0.10% | 0.01 | |
| Al2O3 | 18.75% | 1.17 | |
| SiO2 | 70.83% | 7.50 | |
| Fe2O3 | 0.10% | - | |
| LOI | 0.42% | n/a | |
| Oxide Weight | 633.63 | ||
| Formula Weight | 636.30 | ||
Available in -100, -63 and -45 micron sizes.
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Minerals |
Kaolinite
The most fundamental clay mineral. This mineral is found in nature in its purest form as kaolin. How |
| Materials |
Feldspar 632
|
| Materials |
Feldspar 661
|
| Materials |
Feldspar 635
|
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |