CKR Clay

Oxide Analysis Formula Tolerance
CaO 0.20% 0.01
MgO 0.30% 0.03
K2O 1.60% 0.06
Na2O 0.20% 0.01
TiO2 1.60% 0.07
Al2O3 30.10% 1.00
SiO2 51.90% 2.93
Fe2O3 1.50% 0.03
H2O 12.50%n/a
Oxide Weight 296.17
Formula Weight 338.48

Notes

Available in 30 mesh size.
A light buff burning fireclay.

Related Information

Links

Materials Goldart
A plastic buff burning clay, often used as a major ingredient in stoneware clay bodies.
Materials Industrial Fireclay
Materials Bonding Clay
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

Data

Pyrometric Cone Equivalent 31

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy