1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Plainsman Troy Clay

Description: Kaolin, Halloysite

Oxide Analysis Formula Tolerance
CaO 0.21% 0.01
K2O 0.64% 0.02
MgO 0.18% 0.01
Na2O 0.05% -
TiO2 1.17% 0.05
Al2O3 32.70% 1.00
P2O5 0.04% -
SiO2 48.39% 2.51
Fe2O3 1.04% 0.02
MnO 0.01% -
LOI 14.49%n/a
Oxide Weight 263.34
Formula Weight 307.97

Notes

A material with kaolin-like properties. It contains some halloysite and because of this it has a high fired shrinkage and required a higher percentage of water to make it plastic.

This material is available in bulk raw or powdered to 100 mesh.

Trace Elements:
Ba 380 ppm
Sr 28 ppm
Y 48 ppm
Sc 23 ppm
Zr 350 ppm
Be 2 ppm
V 116 ppm

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.
Minerals Halloysite
From a purely physical properties point-of-view, halloysite is a clay mineral similar to kaolin in f

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy