Digitalfire is facing a takedown order from Plainsman Clays. They are revoking permission to "use any Plainsman content" "on any platform". This is broad and vague enough, and this site large enough, that I am unable to comply or even interpret it in the short timeframe (June 27). Please don't panic, I am overwhelmed by the unbelievable support I am getting. We just need to get them to relent on this demand and call off the lawyer (to at least permit commentary). There are lots of backup sites (many people have the API endpoints), don't start downloading or scraping again and overload the server.

Insight-live.com general operation is not affected by this.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

C & C Ball Clay

Alternate Names: C&C Ball Clay, C and C Ball Clay

Description: White burning plastic ball clay

Oxide Analysis Formula Tolerance
CaO 0.10% 0.01
K2O 0.41% 0.02
MgO 0.20% 0.02
Na2O 0.20% 0.01
TiO2 1.64% 0.08
Al2O3 26.29% 1.00
SiO2 59.84% 3.86
Fe2O3 0.92% 0.02
LOI 10.40%n/a
Oxide Weight 347.63
Formula Weight 387.98

Notes

Considered by some as a stoneware clay, it fires very white and is used in white firing porcelains and stoneware for its excellent plasticity.
The company describes it as a fine-grained engineered blend, well known for its excellent plasticity and fired properties. This consistent blend is suitable for a wide variety of forming processes, where a high degree of plasticity is required, such as dry pressing, jiggering, ram pressing and casting.

Related Information

Links

Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy