Alternate Names: BN
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Alumina
|
| Materials |
Silicon Carbide
|
| Materials |
Boron Carbide
|
| Typecodes |
Abrasive Resistant Super Hard Material
These materials are generally available in granular form, the particles are cemented together using frits to produce abrasive products. However, powdered and slurried forms of these materials can also be formed and fired by various means to produce hard materials. |
| Typecodes |
Non-Oxide Material
Many of these materials are not used in traditional ceramics but they have such incredible properties that some have been included in this database. |
| URLs |
http://en.wikipedia.org/wiki/Boron_nitride
Boron Nitride at Wikipedia |
| Glossary |
Deflocculation
Deflocculation is the magic behind the ceramic casting process, it enables slurries having impossibly low water contents and ware having amazingly low drying shrinkage |
| Glossary |
Hot Pressing
|
| Glossary |
Slip Casting
A method of forming ceramics. A deflocculated (low water content) slurry is poured into absorbent plaster molds. As it sits in the mold, usually 10+ minutes, a layer builds against the mold walls. When thick enough the mold is drained. |