#11 Clay

Oxide Analysis Formula Tolerance
CaO 1.20% 0.07 3
K2O 4.00% 0.13 1
MgO 0.60% 0.05
Na2O 0.30% 0.01
TiO2 1.00% 0.04
Al2O3 33.54% 1.00
SiO2 51.20% 2.59
Fe2O3 1.10% 0.02
LOI 9.18%n/a
Oxide Weight 282.64
Formula Weight 311.21

Related Information

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
Oxides Sm2O3 -

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy