V15098

Alternate Names: V 15098,V-15098

Description: Alkali-Zink-Bor

Oxide Analysis Formula Tolerance
CaO 0.28% 0.41
K2O 0.35% 0.31
ZnO 0.28% 0.28
B2O3 0.16% 0.19
SiO2 3.16% 4.33
Oxide Weight 348.25
Formula Weight 348.25

Related Information

Links

Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 70
Frit Softening Point 655C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy