Stain 6908

Description: STAIN FLUX (PbBSi)

Notes

Old Number: 8
Using stains as underglazes may rob the glaze of its flux causing crawling or dry spots. To alleviate this problem use 10% flux to 90% stain in most situations. For pinks and browns, use a 15:85 ratio.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy