Stain (grey)

Description: Grey (MoAl)

Notes

Molybdenum-alumina greys are produced from calcined mixtures of molybdenum oxide, alumina and zinc oxide.

Color
-----
Neutral grey.

Specific Gravity
----------------
Approximately 4.0

Stability/Kiln Atmosphere
-------------------------
Stable at temperatures up to 1450C.

Will tolerate some reducing atmosphere.

Compatibility
-------------
Suitable for blending with all other types of body or engobe stains to give intermediate shades.

Cost
----
Relatively low.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy