Description: Brown Stains (FeCrZnAl, FeCr, FeCrZn)
| Oxide | Analysis | Formula | Tolerance |
|---|
| Materials |
Stain
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Glaze Color | The host glaze should contain from 3-5% zinc to support the red side of the stain (to get a red-brown color). |
|---|