Description: Spodumene Concentrate

Oxide Analysis Formula Tolerance
CaO 0.05% -
Li2O 7.60% 0.98
K2O 0.08% -
Na2O 0.15% 0.01
P2O5 0.17% -
TiO2 0.01% -
Al2O3 26.50% 1.00
SiO2 64.50% 4.12
Fe2O3 0.07% -
MnO 0.02% -
LOI 0.20%n/a
Oxide Weight 380.77
Formula Weight 381.54

Notes

This is a lithium concentrate, not a commercial product. Talison Lithium primarily produces hard-rock lithium mineral concentrates (spodumene) at its Greenbushes mine in Western Australia. The company extracts and processes raw ore into two main categories of lithium concentrate and sells them directly to customers rather than producing refined lithium chemicals itself.
Technical-Grade Lithium Concentrates Features: Low iron content.Uses: Manufacture of ceramics, specialty glass, and heat-proof cookware.
Chemical-Grade Lithium Concentrates Features: High-yielding lithium mineral concentrate.Uses: Processed further into lithium chemicals (such as lithium hydroxide and lithium carbonate) to power lithium-ion batteries in electric vehicles, laptops, and mobile phones, as well as large energy grid storage systems.

Related Information

Links

Materials Spodumene Concentrate
Materials Foote Spodumene
Materials Spodumene
Spodumene is a lithium sourcing feldspar, an alternative to lithium carbonate to supply Li2O to ceramic glazes. Contains up to about 8% Li2O.
Materials Australian Spodumene
Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

Data

Hardness (Moh) 6-5-7
Frit Softening Point 1420C
Sieve Analysis Dry Tyler 65 mesh: 4% 200 mesh: 80%
Density (Specific Gravity) 3.2

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy