| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.40% | 0.04 | |
| K2O | 5.89% | 0.37 | |
| Na2O | 6.20% | 0.59 | |
| TiO2 | 0.08% | 0.01 | |
| Al2O3 | 18.49% | 1.07 | |
| SiO2 | 68.47% | 6.72 | |
| Fe2O3 | 0.27% | 0.01 | |
| LOI | 0.20% | n/a | |
| Oxide Weight | 588.25 | ||
| Formula Weight | 589.43 | ||
When substituting this for other feldspars, like Minspar, Custer or G200 HP note that the iron content in this one is quite a bit more. So colors could be different.
| Minerals |
Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |