| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 45.50% | 2.03 | |
| Al2O3 | 38.00% | 1.00 | |
| TiO2 | 1.65% | 0.06 | |
| Fe2O3 | 0.90% | 0.02 | |
| CaO | 0.25% | 0.01 | |
| MgO | 0.06% | - | |
| K2O | 0.06% | - | |
| Na2O | 0.04% | - | |
| LOI | 13.40% | n/a | |
| Oxide Weight | 232.08 | ||
| Formula Weight | 267.99 | ||
The data sheet claims this increases strength and plasticity in plastic forming and extrusion operations. Also ideal for blunging to slurries, filter pressing and extrusion, mulling prior to extrusion and spray drying. In all applications, the rapid-pick up and equilibration of process fluids with these clays help minimize batching and blending time.
D-6 D-10 SK-75
Dry M.O.R. @ 230F: 650 1000 250 lbf/in2
SSA: 17.0 19.6 6.5 m2/g
| Materials |
Prestige D-6 Kaolin
|
| URLs |
https://digitalfire.com/4sight/datasheets/PrestigeKaolin.pdf
Covia Prestige Kaolin data sheet |