Prestige D-6 Kaolin

Oxide Analysis Formula Tolerance
SiO2 45.70% 2.03
Al2O3 38.30% 1.00
TiO2 1.48% 0.05
Fe2O3 0.64% 0.01
CaO 0.32% 0.02
MgO 0.07% -
K2O 0.22% 0.01
Na2O 0.01% -
LOI 13.50%n/a
Oxide Weight 231.00
Formula Weight 267.06

Notes

The data sheet claims this increases strength and plasticity in plastic forming and extrusion operations. Also ideal for blunging to slurries, filter pressing and extrusion, mulling prior to extrusion and spray drying. In all applications, the rapid-pick up and equilibration of process fluids with these clays help minimize batching and blending time.

D-6 D-10 SK-75
Dry M.O.R. @ 230F: 650 1000 250 lbf/in2
SSA: 17.0 19.6 6.5 m2/g

Related Information

Links

URLs https://digitalfire.com/4sight/datasheets/PrestigeKaolin.pdf
Covia Prestige Kaolin data sheet
Materials Prestige D-10 Kaolin
Materials Prestige SK-75 Kaolin

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy