Potclays Frit 2270

Alternate Names: 2270 Hvit zircon Boraks fritte, Potclays White Zircon Borax Frit

Description: White Zircon Frit

Oxide Analysis Formula Tolerance
CaO 5.47% 0.41
MgO 1.06% 0.11
ZrO2 12.38% 0.43
Na2O 6.06% 0.41
Al2O3 5.68% 0.24
B2O3 13.58% 0.83
SiO2 54.60% 3.85
ZnO 1.17% 0.06
Oxide Weight 423.87
Formula Weight 423.87

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3302-D
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy