1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Potassium Chromate

Formula: K2CrO4

Oxide Analysis Formula Tolerance
K2O 48.50% 1.00
Cr2O3 51.50% 0.66
Oxide Weight 194.23
Formula Weight 194.23

Notes

A soluble crystalline bright yellow powder. It is used to introduce Chromium oxide into low temperature glazes to achieve colors such as red. The chromium is more effectively dispersed because it is combined with potassium.

Related Information

Links

Materials Potassium Dichromate
Hazards Chromium Compounds Toxicology
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc13/icsc1371.htm
Potassium Dichromate at ilo.og

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy