Pfizer Wollastonite

Description: No longer produced

Oxide Analysis Formula Tolerance
SiO2 50.90% 1.01
CaO 46.90% 1.00
Fe2O3 0.55% -
Al2O3 0.25% -
MgO 0.10% -
TiO2 0.05% -
LOI 0.90%n/a
Oxide Weight 117.77
Formula Weight 118.84

Related Information

Links

Materials Wollastonite
A source of CaO in glazes and a porcelain body material.
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.

Data

Pyrometric Cone Equivalent 18

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy