Alternate Names: Frit PB1V48
Description: Leaded cadmium frit for orage/red colors cone 08-06
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.80% | 0.05 | |
| CdO | 3.70% | 0.10 | |
| K2O | 1.50% | 0.06 | |
| Na2O | 9.50% | 0.53 | |
| PbO | 17.20% | 0.27 | |
| ZrO2 | 0.60% | 0.02 | |
| B2O3 | 14.80% | 0.74 | |
| Al2O3 | 3.10% | 0.11 | |
| SiO2 | 47.00% | 2.70 | |
| Oxide Weight | 339.46 | ||
| Formula Weight | 339.46 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
General Frit GF-25
|
| Materials |
Fusion Frit FL-31
|
| Materials |
Pemco Frit Pb-2G12
|
| Materials |
Ferro Frit 3600
|
| Materials |
Ferro Frit 3548
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.70 |
|---|---|
| Frit Softening Point | 1742F |