Alternate Names: Frit FL31
Description: Cadmium frit for cadmium/selenium class colors
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.80% | 0.05 | |
| K2O | 1.50% | 0.06 | |
| Na2O | 9.50% | 0.53 | |
| CdO | 3.70% | 0.10 | |
| PbO | 17.20% | 0.27 | |
| Al2O3 | 3.10% | 0.11 | |
| B2O3 | 14.80% | 0.74 | |
| SiO2 | 47.00% | 2.70 | |
| ZrO2 | 0.60% | 0.02 | |
| Oxide Weight | 339.46 | ||
| Formula Weight | 339.46 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Pemco Frit PB-1V48
|
| Typecodes |
Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Glaze Color | Lead cadmium frits are available as a base to create classic cadmium selenium colors that cannot be easily achieved in other ways. These glazes can be toxic to work with and the glazed ware will likely leach cadmium. |
|---|---|
| Glaze Color | Lead cadmium frits are available as a base to create classic cadmium selenium colors that cannot be easily achieved in other ways. These glazes can be toxic to work with and the glazed ware will likely leach cadmium. |
| Glaze Color | Lead cadmium frits are available as a base to create classic cadmium selenium colors that cannot be easily achieved in other ways. These glazes can be toxic to work with and the glazed ware will likely leach cadmium. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk