Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-1409

Alternate Names: Frit 1409, Frit P1409

Description: Low expansion high magnesia alkali-free leadless glaze frit

Oxide Analysis Formula Tolerance
CaO 2.20% 0.13
MgO 10.40% 0.87
B2O3 29.00% 1.40
Al2O3 14.40% 0.47
SiO2 44.00% 2.46
Oxide Weight 336.38
Formula Weight 336.38

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 4GF151B
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 4.7x10-6 (50-450C)
Frit Melting Range (C) 1750-1850F
I.F.P. (celsius) 694C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy