P30 Quartz

Oxide Analysis Formula Tolerance
CaO 0.02% 0.08
K2O 0.08% 0.19
TiO2 0.01% 0.03
Al2O3 0.45% 1.00
SiO2 99.20% 374.13
Fe2O3 0.03% 0.04
LOI 0.20%n/a
Oxide Weight 22,619.07
Formula Weight 22,664.40

Related Information

Links

Minerals Quartz
Quartz is the most abundant mineral on earth, it is the main crystalline mineral form of silica (SiO
Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

Data

Bulk Density g/cc (Packed) 1.2
Hardness (Moh) 7
Ultimate Particle Size Distribution >30 micron: 1.5%
Density (Specific Gravity) 2.6
pH for dry powder 8-9