OSML Ball Clay

Notes

A Ball Clay blend designed for use in the sanitaryware industry. Both Kentucky and Tennessee clays are used to create a product that would supply the entire Ball Clay portion of the body. The blend exhibits very good green strength while maintaining excellent casting properties.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Ball Clay
A fine particled highly plastic secondary clay used mainly to impart plasticity to clay and porcelain bodies and to suspend glaze, slips and engobe slurries.
Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy