Mondre and Manz Frit 4067

Description: Barium zinc potash low alumina leaded frit

Oxide Analysis Formula Tolerance
BaO 37.77% 0.50
K2O 4.64% 0.10
Na2O 0.03% -
ZnO 12.03% 0.30
PbO 10.89% 0.10
Al2O3 5.03% 0.10
SiO2 29.61% 1.00
Oxide Weight 202.96
Formula Weight 202.96

Notes

Used in crystalline glazes, it crystallizes on cooling.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Degussa Frit 90420
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy