Formula: MoO3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MoO3 | 100.00% | 1.00 | |
| Oxide Weight | 143.94 | ||
| Formula Weight | 143.94 | ||
Lowers surface tension of melts and thus can be used to encourage crystal development (i.e. with titanium), variegate colorants, impart silvery coloration, opacify. Also used in yellow stains and as a color stabilizer and in lustres to add gold coloration. It is generally a weak influence in these areas.
MoO3 can varporize and have effects on other glazes.