Description: Unknown
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 1.30% | 0.02 | |
| Al2O3 | 0.30% | - | |
| K2O | 0.40% | - | |
| MgO | 19.90% | 0.46 | |
| CaO | 32.00% | 0.53 | |
| LOI | 46.00% | n/a | |
| Oxide Weight | 50.45 | ||
| Formula Weight | 93.42 | ||
| Materials |
Dolomite
An inexpensive source of MgO and CaO for ceramic glazes, also a highly refractory material when fired in the absence of reactant fluxes. |
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |