Iron Sulfate

Alternate Names: Iron(II) Sulphate, Iron(II) Sulfate

Formula: FeSO4

Oxide Analysis Formula Tolerance
Fe2O3 57.50% 1.00
LOI 42.50%n/a
Oxide Weight 160.00
Formula Weight 278.26

Related Information

Links

Materials Spanish Red Iron Oxide
Materials Iron Oxide Red
Red iron oxide is the most common colorant used in ceramic bodies and glazes. As a powder, it is available in red, yellow, black and other colors.
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy