Hommel Frit 529

Description: Leadless high sodium low alumina low boron frit

Oxide Analysis Formula Tolerance
CaO 5.80% 0.26
K2O 2.10% 0.06
Na2O 16.70% 0.68
B2O3 2.60% 0.09
Al2O3 4.00% 0.10
SiO2 68.80% 2.90
Oxide Weight 253.14
Formula Weight 253.14

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3110
High sodium, high thermal expansion low boron frit. A super-feldspar in clay bodies. Melts at very low temperatures. Useful to make crackle glazes.
Materials Keramikos Fritte 31.10
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 9.6 x 10-6 (50-450C)
Co-efficient of Linear Expansion 9.6 x 10-6
Frit Melting Range (C) 1400F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy