Description: Leadless zinc high boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 4.35% | 0.18 | |
| Na2O | 10.66% | 0.40 | |
| ZnO | 14.82% | 0.42 | |
| B2O3 | 28.73% | 0.96 | |
| SiO2 | 41.44% | 1.60 | |
| Oxide Weight | 231.73 | ||
| Formula Weight | 231.73 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3824
|
| Materials |
Pemco Frit P-1733
|
| Materials |
General Frit GF-100
|
| Materials |
Fusion Frit FZ-16
The champion in our frit melt-off competitition. This frit showcases the amazing fluxing power of boron and zinc working together. It is 15.5% ZnO. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk