Description: Leadless barium frit

Oxide Analysis Formula Tolerance
BaO 27.70% 0.67
Na2O 5.50% 0.33
B2O3 12.34% 0.66
Al2O3 5.40% 0.20
SiO2 49.05% 3.03
Oxide Weight 371.16
Formula Weight 371.16

Related Information

Links

Materials General Frit GF-129
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3289
Materials Pemco Frit P-626
Materials Fusion Frit F-65
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.90
Co-efficient of Linear Expansion 7.9 x 10-6
Frit Softening Point 1570F
Frit Melting Range (C) 1570F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy