General Frit GF-129

Alternate Names: Frit 129, Frit GF129

Description: High barium borosilicate leadless frit

Oxide Analysis Formula Tolerance
BaO 26.51% 0.66
Na2O 5.52% 0.34
B2O3 12.40% 0.68
Al2O3 5.34% 0.20
SiO2 50.23% 3.19
Oxide Weight 381.74
Formula Weight 381.74

Related Information

Links

Materials Pemco Frit P-626
Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 400
Materials Ferro Frit 3289
Hazards Barium Carbonate in Glazes
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 6.80
Frit Softening Point 1750F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy